optibond.ru создан как площадка для обмена глубоким клиническим опытом

A novel method to assess the interfacial fracture toughness of two universal resin cements to dentin.

Original PubMed abstract — English. No translation or clinical interpretation.

Authors

Tony Lorey; Jennifer Woolford; Markus B Blatz; Ulrich Lohbauer; Renan Belli; José Ignacio Zorzin

Publication details

Dental materials : official publication of the Academy of Dental Materials · 2026 · Vol. 42 · No. 4 · Pages/article no. 607-617

Publication date (as recorded): 2026-03-31

PMID: 41390292

Abstract (original)

The purpose of this study was to evaluate the adhesion potential of two universal resin cements compared to a gold standard adhesive system, considering application mode and storage time, using a novel method for interfacial fracture toughness (iFT). OBJECTIVE OBJECTIVE

iFT was measured using the Chevron-Notched Beam (CNB) method with a novel modified split-CNB sandwich specimen design. One hundred human third molars were sectioned into enamel-dentin rods, adhesively conditioned, notched, and cut apart in the dentin area. Specimens were bonded using the universal luting resin in self-adhesive mode or with their corresponding adhesive system/primer (RelyX Universal and Scotchbond Universal Plus, Solventum; GCem One and Adhesive Enhancing Primer, GC Corp.). A gold standard adhesive (OptiBond FL, Kerr) in combination with a flowable resin composite as luting material (x-tra base Universal, VOCO) served as a control. The influence of storage time (24 h vs. 180 days), application mode (adhesive vs. self-adhesive), and the material itself on the iFT measured as fracture toughness in mode I (K) according to ASTM C1421-10 was evaluated. Scanning electron microscopy (SEM) was employed to analyze interfacial characteristics and failure modes. METHODS METHODS Ic

Statistical analysis (Kruskal-Wallis H test with Bonferroni-Holm correction) revealed significant differences in iFT between the groups. Specimens stored for 180 days exhibited lower iFT compared to those stored for 24 h. The adhesive application significantly enhanced iFT relative to the self-adhesive mode. GCem One with Adhesive Enhancing Primer (24 h) exhibited the highest interfacial fracture toughness among all investigated groups. SEM analysis indicated a predominance of adhesive failures at the dentin-resin interface, particularly within the self-adhesive groups. RESULTS RESULTS

The application mode and material significantly influence interfacial fracture toughness. The adhesive-assisted application enhances bond stability, while the self-adhesive approach exhibits lower long-term adhesion. CONCLUSIONS CONCLUSIONS

The use of universal resin cements along with their adhesive system/primer significantly enhances adhesion between the tooth and the restoration, leading to improved long-term clinical success. For restorations without microretention, universal resin cements must be used in combination with their adhesive system/primer. CLINICAL SIGNIFICANCE CONCLUSIONS

Source: https://pubmed.ncbi.nlm.nih.gov/41390292/


Rubberdamology
Глобальный аудит

Глобальное сравнение адгезивных систем: IV, V, VI, VII, VIII поколений

Масштабный академический синопсис доказательной базы PubMed. Сравнительный анализ устойчивости гибридного слоя к гидролизу, физика «водных деревьев» в упрощенных бондах и обоснование тотального превосходства многокомпонентного запечатывания дентина в рамках стандартов RSBC.

OptiBond FL
Глобальный аудит

Полный реестр научных статей о применении OptiBond FL

Массив в 401 исследование по OptiBond FL — это колоссальный объем данных, который наглядно объясняет, почему этот материал официально признан мировым научным сообществом «золотым стандартом» адгезии (Dreweck et al., PMID: 34919728; Peumans et al., PMID: 37435814).

Поделиться этой информацией
URL публикации
Предыдущая публикация

Dual cure activator improves bond performance of etch-and-rinse mode universal adhesives to bleached enamel.

Следующая публикация

Effect of surface conditioning and adhesive strategies on the repair bond strength of resin matrix ceramics.

Добавить комментарий

Ваш адрес email не будет опубликован. Обязательные поля помечены *

Смотреть далее