Enamel Deproteinization with Sodium Hypochlorite: Effects on Ceramic Bracket Bond Strength.

Original PubMed abstract — English. No translation or clinical interpretation.

Authors

Priscila Cordeiro; José Guilherme Neves; Midori Tsuzuki; Anália Gabriela Ferraz Facury; Lourenço Correr-Sobrinho; Ana Rosa Costa

Publication details

Brazilian dental journal · 2025 · Vol. 36 · Pages/article no. e246106

Publication date (as recorded): 2024-12-31

PMID: 40243868

Abstract (original)

To assess the efficiency of different concentrations of sodium hypochlorite (NaOCl) on the bonding of ceramic brackets to dental enamel using different bonding protocols. Ceramic, a polycrystalline bracket, was bonded to 90 extracted bovine incisors using primer + Transbond XT (P+TXT); Optibond S adhesive + Transbond XT (OS+TXT), and OS + Orthocem (OS+OC). Three concentrations of NaOCl (0%, 2.5%, and 5.25%) were used for each material, resulting in nine experimental groups (n=10). The shear bond strength (SBS) assay was performed on a universal testing machine. The surface morphology of the enamel and tooth/bonding material interface was examined under a scanning electron microscope. Kruskal-Wallis and Dunn's tests were performed to compare the non-parametric data (ARI scores). SBS data were analyzed using a generalized linear model. All analyses were performed using the R program and with a significance level of 5%. No significant differences in SBS between the groups with different concentrations of NaOCl (p>0.05). OS+OC group yielded the lowest bond strength values (3.35 MPa_0%, 4.90 MPa_2.5%, 4.68 MPa_5.25%) compared to the other groups, regardless of NaOCl (p<0.05). No significant difference between the materials regarding the ARI score (p>0.05). OS+TXT-5.25% showed significantly higher scores (14.4 MPa) than OS+TXT-2.5% (9.17 MPa) (p<0.05). The surface morphology analysis revealed a change in the etching pattern for types 1 and 2 when NaOCl was used. The different concentrations of NaOCl previously applied onto the enamel surface did not enhance bond strength. OS+OC should not be recommended for bonding with fixed ceramic orthodontic devices.

Source: https://pubmed.ncbi.nlm.nih.gov/40243868/


Rubberdamology
Глобальный аудит

Глобальное сравнение адгезивных систем: IV, V, VI, VII, VIII поколений

Масштабный академический синопсис доказательной базы PubMed. Сравнительный анализ устойчивости гибридного слоя к гидролизу, физика «водных деревьев» в упрощенных бондах и обоснование тотального превосходства многокомпонентного запечатывания дентина в рамках стандартов RSBC.

OptiBond FL
Глобальный аудит

Полный реестр научных статей о применении OptiBond FL

Массив в 401 исследование по OptiBond FL — это колоссальный объем данных, который наглядно объясняет, почему этот материал официально признан мировым научным сообществом «золотым стандартом» адгезии (Dreweck et al., PMID: 34919728; Peumans et al., PMID: 37435814).

Поделиться этой информацией
URL публикации
Предыдущая публикация

Shear bond strength of universal adhesives to human enamel and dentin.

Следующая публикация

Effects of Endodontic Irrigants on Shear Bond Strength of Mild Universal Adhesives to Dentin.

Добавить комментарий

Ваш адрес email не будет опубликован. Обязательные поля помечены *

Смотреть далее