Shear Bond Strength of Adhesives Placed following Selective Removal of Red-Fluorescing Carious Dentine in vitro.

Original PubMed abstract — English. No translation or clinical interpretation.

Authors

Áine M Lennon; Nina Sophie Reich; Gerlinde Ferstl; Helga Ebensberger; Karl-Anton Hiller; Wolfgang Buchalla

Publication details

Caries research · 2024 · Vol. 58 · No. 1 · Pages/article no. 17-29

Publication date (as recorded): 2023-12-31

PMID: 37797597

Abstract (original)

Red-fluorescing dentine indicates bacterial contamination [Caries Res 2002; 36: 315-319]. We investigated effect of removal of red fluorescent dentine caries on shear bond strength and fracture mode of 4 adhesive approaches. Sixty-five carious teeth and 50 noncarious controls were distributed into 4 groups: Clearfil™ self-etch (CSE), OptiBond™ FL total etch (OTE), Scotchbond™ Universal total etch (STE) and self-etch (SSE). Samples were excited at 405 nm and viewed through 530 nm filter. Carious samples were ground flat exposing strongly red-fluorescing (StrongRF) dentine, on which a composite cylinder was placed, using one of 4 adhesives. After 22 h in water, shear bond strength and fracture mode were analysed. StrongRF was removed; composite cylinders were placed on weakly red-fluorescing (WeakRF) dentine and tested as described above. Finally, red-fluorescing dentine was removed, and composite cylinders were placed on non-fluorescing (NonRF) dentine and tested. Composites were placed at 3 corresponding heights in controls. After 22 h in water, shear bond strength testing and fracture mode analysis were performed. Differences were tested using Mann-Whitney or Wilcoxon tests (p ≤0.05). Median (Q1, Q3) shear bond strength on StrongRF was SSE 14.4 (9.2, 18.2) MPa >CSE 10.2 (6.4, 17.3) MPa >STE 9.1 (6.9, 11.2) MPa >OTE 6.8 (4.0, 10.8) MPa. Shear bond strength increased statistically significantly for all adhesives on WeakRF: SSE 19.8 (13.6, 24.3) MPa >STE 19.5 (12.7, 23.1) MPa >CSE 17.5 (12.0, 22.5) MPa >OTE 15.8 (11.9, 20.9) MPa. Only STE 25.6 (22.4, 29.1) MPa and CSE 22.1 (17.6, 24.6) MPa were significantly different on NonRF compared to WeakRF. For controls tested at corresponding depths, superficial shear bond strength was OTE 18.7 (16.0, 22.1) MPa >STE 18.4 (12.0, 25.9) MPa >CSE 18.1 (12.7, 20.7) MPa >SSE 13.0 (9.6, 17.8) MPa. This was significantly higher compared to StrongRF except for SSE. Central shear bond strength was not significantly different to WeakRF, deep shear bond strength was significantly lower for SSE and CSE but higher for OTE compared to carious. Conclusion: StrongRF dentine should be removed for higher shear bond strength, but WeakRF dentine can often be preserved without compromising adhesive bond strength.

Source: https://pubmed.ncbi.nlm.nih.gov/37797597/


Rubberdamology
Глобальный аудит

Глобальное сравнение адгезивных систем: IV, V, VI, VII, VIII поколений

Масштабный академический синопсис доказательной базы PubMed. Сравнительный анализ устойчивости гибридного слоя к гидролизу, физика «водных деревьев» в упрощенных бондах и обоснование тотального превосходства многокомпонентного запечатывания дентина в рамках стандартов RSBC.

OptiBond FL
Глобальный аудит

Полный реестр научных статей о применении OptiBond FL

Массив в 401 исследование по OptiBond FL — это колоссальный объем данных, который наглядно объясняет, почему этот материал официально признан мировым научным сообществом «золотым стандартом» адгезии (Dreweck et al., PMID: 34919728; Peumans et al., PMID: 37435814).

Поделиться этой информацией
URL публикации
Предыдущая публикация

Curing modes affects micro-tensile bond strength and durability of dual curing resin cements to dentin.

Следующая публикация

Effect of Modified Triple-Layer Application on the Bond Strength of Different Dental Adhesive Systems to Dentin.

Добавить комментарий

Ваш адрес email не будет опубликован. Обязательные поля помечены *

Смотреть далее