OCT for evaluation of a universal adhesive in a three-year clinical trial.

Original PubMed abstract — English. No translation or clinical interpretation.

Authors

Rainer Haak; Matthias Häfer; Ellen Schulz-Kornas; Tobias Meißner; Hartmut Schneider

Publication details

Journal of dentistry · 2026 · Vol. 177 · Pages/article no. 107106

Publication date (as recorded): 2026-10-14

PMID: 42880480

Abstract (original)

In parallel with the 36-month clinical evaluation of a universal adhesive, tooth-composite bond failure was assessed by tomography. OBJECTIVES OBJECTIVE

In 55 patients, three non-carious cervical lesions (NCCLs) each were restored with Filtek™ Supreme XTE (3 M) using the universal adhesive Scotchbond™ Universal Adhesive (SBU, 3 M) in the self-etch (SE) or selective enamel-etch (SEE) mode or by OptiBond™ FL (OFL, Kerr, reference, randomization). Immediately after restoration placement (T0) and in parallel with the clinical assessments (FDI criteria) at 6, 12, 24, and 36 months (M), the restorations were imaged by optical coherence tomography (OCT) to quantify interfacial adhesive defects (ADs; 14 days, clinical only). Cumulative failure rates (CFRs) and means of ADs were statistically analyzed. METHODS METHODS

From six to 36M, CFRs were lower in the SBU groups vs. OFL (p ≤ 0.004). Compared to SBU-SE or OFL, SBU-SEE resulted in reduced marginal staining (≥ 12M; p: 0.002 — 0.727) and increased marginal adaptation (≥ 12M; p: 0.001 — 0.629). Increased ADs appeared on the enamel with SBU-SE vs. SBU-SEE and OFL (T0 — 36M; p ≤ 0.001/0.048) and with OFL vs. SBU-SEE (≥ 6M; p ≤ 0.025). At dentin/cement less defects appeared using SBU-SEE vs. SBU-SE (≥ 6M) or OFL (≥ T0, p ≤ 0.0115), and fewer in the SBU-SE vs. OFL group (≥ T0, p ≤ 0.001). Before restoration loss, the adhesive defects on the dentin/cement were increased (p ≤ 0.05). RESULTS RESULTS i i i i i i i i

Clinical assessments and OCT-based analyses were consistent. In terms of bond failure, however, the groups already differed upon restoration placement, with reproducible substrate-specific differences becoming apparent. CONCLUSIONS CONCLUSIONS

The universal adhesive Scotchbond™ Universal Adhesive in SEE mode performed most favorably. Interfacial adhesive defects detectable by OCT reliably predict the performance of a restoration system. #DRKS00011084, http://www.drks.de/DRKS00011084, 30.09.2016. CLINICAL SIGNIFICANCE CONCLUSIONS

Source: https://pubmed.ncbi.nlm.nih.gov/42880480/


Rubberdamology
Глобальный аудит

Глобальное сравнение адгезивных систем: IV, V, VI, VII, VIII поколений

Масштабный академический синопсис доказательной базы PubMed. Сравнительный анализ устойчивости гибридного слоя к гидролизу, физика «водных деревьев» в упрощенных бондах и обоснование тотального превосходства многокомпонентного запечатывания дентина в рамках стандартов RSBC.

OptiBond FL
Глобальный аудит

Полный реестр научных статей о применении OptiBond FL

Массив в 401 исследование по OptiBond FL — это колоссальный объем данных, который наглядно объясняет, почему этот материал официально признан мировым научным сообществом «золотым стандартом» адгезии (Dreweck et al., PMID: 34919728; Peumans et al., PMID: 37435814).

Поделиться этой информацией
URL публикации
Предыдущая публикация

Comparative Analysis of Bond Strength in Endodontic Access: Immediate Endodontic Sealing Versus Delayed Endodontic Sealing.

Следующая публикация

The Effect of Different Types of Adhesive Systems on Marginal Integrity of Class II Resin Composite Restoration.

Добавить комментарий

Ваш адрес email не будет опубликован. Обязательные поля помечены *

Смотреть далее