Abstract (original)

This study evaluated the effects of different provisional luting cement removal methods on the shear bond strength (SBS) of resin cement to dentin following immediate dentin sealing (IDS) performed with two adhesive systems. A total of 168 extracted, caries-free human third molars were used, of which 144 were allocated for SBS testing and 24 for scanning electron microscopy (SEM) analysis. Specimens were assigned according to the IDS protocol (no IDS, IDS with OptiBond FL, or IDS with G2-Bond), followed by provisional cementation using an eugenol-free temporary cement. Contaminated surfaces were subsequently cleaned with a hand scaler, aluminum oxide (AlO) air abrasion, or Katana Cleaner prior to final bonding with a dual-cure resin cement. SBS was measured after 24 h of water storage, and surface morphology was evaluated by SEM at 2500× magnification. IDS significantly increased SBS under uncontaminated conditions, with G2-Bond-based IDS exhibiting higher bond strength values than specimens without IDS. However, provisional cement contamination significantly reduced SBS regardless of the cleaning method applied, and none of the tested protocols fully restored the bond strength observed in uncontaminated IDS-treated dentin. SEM analysis revealed residual cement remnants and surface alterations after cleaning, even in specimens that appeared macroscopically clean. Within the limitations of this in vitro study, IDS enhances resin-dentin bonding when contamination is avoided; however, current mechanical and chemical cleaning methods are insufficient to completely recover bond strength compromised by provisional cement contamination, highlighting the importance of preventing contamination and preserving IDS layer integrity during indirect restorative procedures. 2 3

Source: https://pubmed.ncbi.nlm.nih.gov/41745560/


Rubberdamology
Глобальный аудит

Глобальное сравнение адгезивных систем: IV, V, VI, VII, VIII поколений

Масштабный академический синопсис доказательной базы PubMed. Сравнительный анализ устойчивости гибридного слоя к гидролизу, физика «водных деревьев» в упрощенных бондах и обоснование тотального превосходства многокомпонентного запечатывания дентина в рамках стандартов RSBC.

OptiBond FL
Глобальный аудит

Полный реестр научных статей о применении OptiBond FL

Массив в 401 исследование по OptiBond FL — это колоссальный объем данных, который наглядно объясняет, почему этот материал официально признан мировым научным сообществом «золотым стандартом» адгезии (Dreweck et al., PMID: 34919728; Peumans et al., PMID: 37435814).

Поделиться этой информацией
URL публикации
Предыдущая публикация

Effect of Immediate Dentin Sealing and Surface Cleansing on Ceramic-to-Dentin Bond Strengths.

Следующая публикация

Investigating the Effect of Saliva Contamination at Different Time Intervals on Micro-Shear Bond Strength of Dentin with Immediate Dentin Sealing.

Добавить комментарий

Ваш адрес email не будет опубликован. Обязательные поля помечены *

Смотреть далее