Abstract (original)

To investigate the influence of filler type/loading on the micro-tensile fracture strength (μTFS) of adhesive resins, as measured 'immediately' upon preparation and after 1-week water storage ('water-stored'). OBJECTIVES

The morphology and particle-size distribution of three filler particles, referred to as 'Glass-S' (Esschem Europe), 'BioUnion' (GC), and 'CPC_Mont', were correlatively characterized by SEM, TEM, and particle-size analysis. These filler particles were incorporated into an unfilled adhesive resin ('BZF-29unfilled', GC) in different concentrations to measure the 'immediate' μTFS. After 1-week water storage, the 'water-stored' μTFS of the experimental particle-filled adhesive resins with the most optimum filler loading, specific for each filler type, was measured. In addition, the immediate and water-stored μTFS of the adhesive resins of three experimental two-step universal adhesives based on the same resin matrix but varying for filler type/loading, coded as 'BZF-21' (containing silica and bioglass), 'BZF-29' (containing solely silica), and 'BZF-29_hv' (highly viscous with a higher silica loading than BZF-29), and of the adhesive resins of the gold-standard adhesives OptiBond FL ('Opti-FL', Kerr) and Clearfil SE Bond 2 ('C-SE2', Kuraray Noritake) was measured along with that of BZF-29unfilled (GC) serving as control/reference. Statistics involved one-way and two-way ANOVA followed by post-hoc multiple comparisons (α<0.05). METHODS

Glass-S, BioUnion, and CPC_Mont represent irregular fillers with an average particle size of 8.5-9.9 μm. Adding filler to BZF-29unfilled decreased μTFS regardless of filler type/loading. One-week water storage reduced μTFS of all adhesive resins except BZF-21, with the largest reduction in μTFS recorded for BZF-29unfilled. Among the three filler types, the μTFS of the 30 wt% Glass-S and 20 wt% BioUnion filled adhesive resin was not significantly different from the μTFS of BZF-29unfilled upon water storage. RESULTS

Adding filler particles into adhesive resin did not enhance its micro-tensile fracture strength but appeared to render it less sensitive to water storage as compared to the unfilled adhesive resin investigated. CONCLUSIONS

Source: https://pubmed.ncbi.nlm.nih.gov/38632849/


Rubberdamology
Глобальный аудит

Глобальное сравнение адгезивных систем: IV, V, VI, VII, VIII поколений

Масштабный академический синопсис доказательной базы PubMed. Сравнительный анализ устойчивости гибридного слоя к гидролизу, физика «водных деревьев» в упрощенных бондах и обоснование тотального превосходства многокомпонентного запечатывания дентина в рамках стандартов RSBC.

OptiBond FL
Глобальный аудит

Полный реестр научных статей о применении OptiBond FL

Массив в 401 исследование по OptiBond FL — это колоссальный объем данных, который наглядно объясняет, почему этот материал официально признан мировым научным сообществом «золотым стандартом» адгезии (Dreweck et al., PMID: 34919728; Peumans et al., PMID: 37435814).

Поделиться этой информацией
URL публикации
Предыдущая публикация

Effects of Endodontic Irrigants on Shear Bond Strength of Mild Universal Adhesives to Dentin.

Следующая публикация

Internal Adaptation of Composite Fillings Made Using Universal Adhesives-A Micro-Computed Tomography Analysis.

Добавить комментарий

Ваш адрес email не будет опубликован. Обязательные поля помечены *

Смотреть далее