Investigating the Effect of Saliva Contamination at Different Time Intervals on Micro-Shear Bond Strength of Dentin with Immediate Dentin Sealing.

Original PubMed abstract — English. No translation or clinical interpretation.

Authors

Salehe Sekandari; Pouria Bashian; Hamideh Sadat Mohammadipour; Ziba Shirkhani Kelagari; Fatemeh Sekandari; Zahra Ari Tabarestani

Publication details

The Saudi dental journal · 2026 · Vol. 38 · No. 4

Publication date (as recorded): 2026-03-23

PMID: 41874772

Abstract (original)

The immediate dentin sealing (IDS) approach involves sealing the dentin immediately after tooth preparation and before impression taking. This in vitro study aimed to investigate the effect of saliva contamination at various time intervals on the micro-shear bond strength (µSBS) of dentin sealed using a three-step etch-and-rinse adhesive. AIM OBJECTIVE

The occlusal coronal third of 40 intact third molars was removed, and IDS was applied using the three-step adhesive OptiBond FL. The bonded samples were divided into four groups and exposed to non-stimulating natural saliva for 0, 7, 14, and 30 days. After saliva exposure, the teeth were rinsed, and the IDS surfaces were conditioned with 50 µm alumina particles for 5 seconds. The standard adhesive procedure was then followed, and resin composite restoration was applied. µSBS was measured using a universal testing machine, and failure modes were recorded. Data were analyzed using Shapiro-Wilk and ANOVA tests (α < 0.05). MATERIALS AND METHODS METHODS

The highest bond strength was observed in the control group (25.32 ± 6.70 MPa), while the lowest was in the group exposed to saliva for 30 days (21.93 ± 3.26 MPa). However, no statistically significant difference was found between the groups (P = 0.308). The predominant failure mode in all samples, except for one specimen in the control group, which exhibited mixed failure, was adhesive. RESULTS RESULTS

Within the limitations of this in vitro study, saliva contamination for up to 30 days did not significantly affect the µSBS of dentin samples sealed using the IDS method. However, long-term clinical trials are needed to confirm these findings. CONCLUSION CONCLUSIONS

Source: https://pubmed.ncbi.nlm.nih.gov/41874772/


Rubberdamology
Глобальный аудит

Глобальное сравнение адгезивных систем: IV, V, VI, VII, VIII поколений

Масштабный академический синопсис доказательной базы PubMed. Сравнительный анализ устойчивости гибридного слоя к гидролизу, физика «водных деревьев» в упрощенных бондах и обоснование тотального превосходства многокомпонентного запечатывания дентина в рамках стандартов RSBC.

OptiBond FL
Глобальный аудит

Полный реестр научных статей о применении OptiBond FL

Массив в 401 исследование по OptiBond FL — это колоссальный объем данных, который наглядно объясняет, почему этот материал официально признан мировым научным сообществом «золотым стандартом» адгезии (Dreweck et al., PMID: 34919728; Peumans et al., PMID: 37435814).

Поделиться этой информацией
URL публикации
Предыдущая публикация

Effects of Provisional Cement Cleaning Methods on Resin-Dentin Bond Strength Following Immediate Dentin Sealing with Different Adhesive Systems.

Следующая публикация

Repair Bond Strength of Ion-Releasing Versus Conventional Resin Composites.

Добавить комментарий

Ваш адрес email не будет опубликован. Обязательные поля помечены *

Смотреть далее