optibond.ru создан как площадка для обмена глубоким клиническим опытом

Filler Mixed Into Adhesives Does Not Necessarily Improve Their Mechanical Properties.

Original PubMed abstract — English. No translation or clinical interpretation.

Authors

C Tang; B Mercelis; F Zhang; C Mocquot; K Nakanishi; K Yoshihara; M Peumans; B Van Meerbeek

Publication details

Operative dentistry · 2024 · Vol. 49 · No. 3 · Pages/article no. 311-324

Publication date (as recorded): 2024-04-30

PMID: 38632849

Abstract (original)

To investigate the influence of filler type/loading on the micro-tensile fracture strength (μTFS) of adhesive resins, as measured 'immediately' upon preparation and after 1-week water storage ('water-stored'). OBJECTIVES

The morphology and particle-size distribution of three filler particles, referred to as 'Glass-S' (Esschem Europe), 'BioUnion' (GC), and 'CPC_Mont', were correlatively characterized by SEM, TEM, and particle-size analysis. These filler particles were incorporated into an unfilled adhesive resin ('BZF-29unfilled', GC) in different concentrations to measure the 'immediate' μTFS. After 1-week water storage, the 'water-stored' μTFS of the experimental particle-filled adhesive resins with the most optimum filler loading, specific for each filler type, was measured. In addition, the immediate and water-stored μTFS of the adhesive resins of three experimental two-step universal adhesives based on the same resin matrix but varying for filler type/loading, coded as 'BZF-21' (containing silica and bioglass), 'BZF-29' (containing solely silica), and 'BZF-29_hv' (highly viscous with a higher silica loading than BZF-29), and of the adhesive resins of the gold-standard adhesives OptiBond FL ('Opti-FL', Kerr) and Clearfil SE Bond 2 ('C-SE2', Kuraray Noritake) was measured along with that of BZF-29unfilled (GC) serving as control/reference. Statistics involved one-way and two-way ANOVA followed by post-hoc multiple comparisons (α<0.05). METHODS

Glass-S, BioUnion, and CPC_Mont represent irregular fillers with an average particle size of 8.5-9.9 μm. Adding filler to BZF-29unfilled decreased μTFS regardless of filler type/loading. One-week water storage reduced μTFS of all adhesive resins except BZF-21, with the largest reduction in μTFS recorded for BZF-29unfilled. Among the three filler types, the μTFS of the 30 wt% Glass-S and 20 wt% BioUnion filled adhesive resin was not significantly different from the μTFS of BZF-29unfilled upon water storage. RESULTS

Adding filler particles into adhesive resin did not enhance its micro-tensile fracture strength but appeared to render it less sensitive to water storage as compared to the unfilled adhesive resin investigated. CONCLUSIONS

Source: https://pubmed.ncbi.nlm.nih.gov/38632849/


Rubberdamology
Глобальный аудит

Глобальное сравнение адгезивных систем: IV, V, VI, VII, VIII поколений

Масштабный академический синопсис доказательной базы PubMed. Сравнительный анализ устойчивости гибридного слоя к гидролизу, физика «водных деревьев» в упрощенных бондах и обоснование тотального превосходства многокомпонентного запечатывания дентина в рамках стандартов RSBC.

OptiBond FL
Глобальный аудит

Полный реестр научных статей о применении OptiBond FL

Массив в 401 исследование по OptiBond FL — это колоссальный объем данных, который наглядно объясняет, почему этот материал официально признан мировым научным сообществом «золотым стандартом» адгезии (Dreweck et al., PMID: 34919728; Peumans et al., PMID: 37435814).

Поделиться этой информацией
URL публикации
Предыдущая публикация

Bond Strength, Microleakage, Microgaps, and Marginal Adaptation of Self-adhesive Resin Composites to Tooth Substrates with and without Preconditioning with Universal Adhesives.

Следующая публикация

Effect of sodium hypochlorite, ethylenediaminetetraacetic acid, and dual-rinse irrigation on dentin adhesion using an etch-and-rinse or self-etch approach.

Добавить комментарий

Ваш адрес email не будет опубликован. Обязательные поля помечены *

Смотреть далее